Skin Panel Defect Troubleshooting

Job ID: 40229885

Budget: ₹12,500 – ₹37,500 INR

During press-tool try-out I keep seeing surface defects on our A-, B- and C-class skin panels. The trouble spots sit right in the aesthetic area, so every flaw is immediately visible. The most common issues are:

• Die marks
• Dents
• Waviness
• Hitting marks

I want someone who can step into the current try-out cycle, pinpoint the root causes, and guide the corrective actions until we reach a class-A finish. Practical press-shop skills—spotting, shimming, polishing—and familiarity with forming-simulation software such as AutoForm or Stampack will help you move quickly.

Deliverables
• Diagnostic report with measurements, defect mapping, and root-cause analysis
• Clear action plan for die re-work or process adjustment
• Hands-on (or remote) support through at least one repeat run
• Final verification parts that meet OEM appearance standards

If you have solved similar skin-panel problems, tell me how you did it and how soon you can start.
Related categories: Manufacturing Strategy Six Sigma